Hi. Did he use grey adhesive?new porcelain floor tiles laid 4 weeks ago over new electric heating matts. Heating only connected a week ago and dark lines showing on most tiles?
possible causes? Any help/ guidance appreciated. Laid by tiler not DIY.
View attachment 114140
YesHi. Did he use grey adhesive?
and that would show through an 8mm porcelain tile?
HiThey are 2 things you have to know, did the tiler cover the underfloor heating with self levelling and he gone for grey adhesive and dot and dab.
It has been known yes , hence why a solid bed is best achieved.. on light tiles no matter the biscuit ( body ) , i use white adhesive.and that would show through an 8mm porcelain tile?
thanks for responses.....don’t know how I would prove tiles were at fault?Might be the quality of the tiles
Thnx. Are lines likely to be permanent? Tiles laid 4 weeks ago UFH only hooked up a week or so ago.It has been known yes , hence why a solid bed is best achieved.. on light tiles no matter the biscuit ( body ) , i use white adhesive.
We had a similar issue on a job. We were brought in to investigate for insurance purposes.new porcelain floor tiles laid 4 weeks ago over new electric heating matts. Heating only connected a week ago and dark lines showing on most tiles?
possible causes? Any help/ guidance appreciated. Laid by tiler not DIY.
View attachment 114140
Thanks for that.We had a similar issue on a job. We were brought in to investigate for insurance purposes.
1.There was no membrane put down onto the new concrete flooring and the moisture came through from the concrete into the grey adhesive and stained the tiles.
2. The tiles weren't fitted correctly many where dot and dabbed there was actually pools of moisture when we lifted the tile.
3. The tiles where laid onto concrete that was new and hadn't been allowed to cure and dry long enough.
Hope this help
It’s the adhesive, sorry but simple as that.Thanks for that.
the kitchen was extended so part old floor part new, there was a DPM but down on new floor,. New floor was a quick set of about a week, but was left for some 6 weeks before anything went down onto it, however the lines are on tiles on both old and new floor so,fairly sure It’s not the floor. I assume that’s a reasonable assumption?
truth hurts! I now have to decide having new tiles ripped up with all the mess involved even more of an issue with electric UFH mats underneath or live with the lines 😱It’s the adhesive, sorry but simple as that.
My guess is that the SLC didn't lose it's required moisture content prior to tiling, and everybody just carried own piling down more stuff and trapping more moisture...new porcelain floor tiles laid 4 weeks ago over new electric heating matts. Heating only connected a week ago and dark lines showing on most tiles?
possible causes? Any help/ guidance appreciated. Laid by tiler not DIY.
View attachment 114140
Really? Most self levelling screed is ok to cover in 24 hours or less. This was screened one morning and tiling did not start till following day and took a further 4 days to complete yet lines are on all tiles pretty much, certainly all full size tileszMy guess is that the SLC didn't lose it's required moisture content prior to tiling, and everybody just carried own piling down more stuff and trapping more moisture...
Put a carpet over it,
Hi, that looks to me like adhesive bleed through the tile. If you look closely enough you can see the lines correspond to the trowel that was used to lay the adhesive. This is due to a couple of reasons.. 1) Grey adhesive used instead of white. 2) No back buttering of the tile prior to laying it onto the adhesive ridges. 3) The adhesive ridges have not been collapsed and that's the lines you can clearly see.new porcelain floor tiles laid 4 weeks ago over new electric heating matts. Heating only connected a week ago and dark lines showing on most tiles?
possible causes? Any help/ guidance appreciated. Laid by tiler not DIY.
View attachment 114140
Yeah, you're probably right, dependant on temp. Are they fully vitrified porcelain tiles?Really? Most self levelling screed is ok to cover in 24 hours or less. This was screened one morning and tiling did not start till following day and took a further 4 days to complete yet lines are on all tiles pretty much, certainly all full size tilesz
.
HiYeah, you're probably right, dependant on temp. Are they fully vitrified porcelain tiles?
I've changed my mind to the incorrect installation of the UFH wires and/or waiting times before it was turned on.
It could be excessive heat due to the UFH installer ordering too much mat and overlaying (not allowable) or a rapid heating of the mat/cable which has caused a premature curing of the background.
How much faith do you hold with the tiler you employed?
They are not cowboys for sure , do a lot of bathrooms especially, and seemed to know what they were doing.Hi
saw the mats down and no overlapping..once UFH turned on was only set at a ro9m temp of 20 degrees, floor temp never much above 14 deg,
he was meticulous with each tile is all I can say , as not had this work done before.
not sure if vitrified as just described as porcelain, was not aware of the term vitrified until recently .
I would run the UFH for a few weeks and see if it improves. Fingers crossed it might.They are not cowboys for sure , do a lot of bathrooms especially, and seemed to know what they were doing.
bit of a nightmare as not sure whether to give it some time fade, they are checking with their adhesive suppler as never had this before.
They are described as glazed porcelain..Hi
saw the mats down and no overlapping..once UFH turned on was only set at a ro9m temp of 20 degrees, floor temp never much above 14 deg,
he was meticulous with each tile is all I can say , as not had this work done before.
not sure if vitrified as just described as porcelain, was not aware of the term vitrified until recently .
thanks, have agreed with tilers that as tiles were laid couple of weeks before heating was hooked up, that would leave till end of March and in meantime they are seeking sone advice from the adhesive suppliers who will probably say the same.I would run the UFH for a few weeks and see if it improves. Fingers crossed it might.
Vitrified means that the tile isn't porous to any problematic level of moisture. Porcelain is a material designed for very low porosity, hence it's outdoor use in cold climates and hard wearing properties.Hi
saw the mats down and no overlapping..once UFH turned on was only set at a ro9m temp of 20 degrees, floor temp never much above 14 deg,
he was meticulous with each tile is all I can say , as not had this work done before.
not sure if vitrified as just described as porcelain, was not aware of the term vitrified until recently .
Keep us updated on results 👍thanks, have agreed with tilers that as tiles were laid couple of weeks before heating was hooked up, that would leave till end of March and in meantime they are seeking sone advice from the adhesive suppliers who will probably say the same.
thanks For you input , appreciated.
Will do and thanksKeep us updated on results 👍