has anyone used kerakoll eco h40 ideal directly onto anhydrite screed? are there any issues?? whats the minimum moisture content before laying on anhydrite?
 
Seen it used loads of times. Not aware of any issues direct to anhydrite provided its sanded and vacuumed well. Moisture needs to be below 0.5% and any underfloor heating must be commissioned and run first...
 
I am told by a Kerakoll stockist that it is a standard setting dispersion adhesive so when used with a decoupling layer it can take a long time to set. Lovely to work with though is what the feedback says.
 
It is a std set and to be honest I'm not sure i would use it with n coupling membrane simply because I do know of a couple of issues where that has been done and the setting time caused a problem.
 
Id rather keraquick and latexplus onto eco prim T primer mixed 1:2 with water after abraiding the floor and hovering.
 
I am told by a Kerakoll stockist that it is a standard setting dispersion adhesive so when used with a decoupling layer it can take a long time to set. Lovely to work with though is what the feedback says.

Yes I heard of someone that had that issue
 

Advertisement

Thread Information

Title
kerakoll h40 eco ideal
Prefix
N/A
Forum
Canada Tile Advice
Start date
Last reply date
Replies
6

Advertisement

Tilers Forums Official Sponsors

UK Tiling Forum; UK

Thread statistics

Created
Unregistered,
Last reply from
Gazzer,
Replies
6
Views
6,784

Thread statistics

Created
Unregistered,
Last reply from
Gazzer,
Replies
6
Views
6,784
Back