N
nudge
I am hoping that some one over there with some more experience with the PCI-"NANOLIGHT" specifically can advise if they are experiencing any problems with the product.
We have stocked and sold the product here in Oz for about 2 years and all seemed to be going very well with great acceptance from the trade and sales volume & word of mouth building towards it becoming one of our largest selling individual adhesive lines. :hurray: However over the last 12 months or so several of our clients are getting complete failures. i.e. tiles coming off in mass, so clean they could be reused, it's like a mould of the tile is left in the adhesive. now i am hereing other stories from other tilers who have also had problems but bought the product elsewhere.😳
I can advise we virtually never have problems here with any of our brands and I am very experienced with the tecnical attributes of other normal brands & products but this is different & none of the common answers as to why it is happening apply & no answers are forthcoming from BASF here who don't normally handle tile & stone adhesives in this country & so are very little help, they are just keeping their fingers crossed that the problem goes away & it was all a big gliche or misunderstanding - but it isn't. :incazzato: and so i am attempted to finally get to the bottom of it for them.
what I can tell you is that in every case whether inside-outside or wall or floor to any substrate & with all tilers & various methods of application the 1 common denominator I can find is, in each case the problem tile has been porcelain - large 300x600 or 600x600 and large notched trowels or back buttering were used to make up for any uneveness in the substrate.
any suggestions will be graciuosly accepted but actual experience would be even better
We have stocked and sold the product here in Oz for about 2 years and all seemed to be going very well with great acceptance from the trade and sales volume & word of mouth building towards it becoming one of our largest selling individual adhesive lines. :hurray: However over the last 12 months or so several of our clients are getting complete failures. i.e. tiles coming off in mass, so clean they could be reused, it's like a mould of the tile is left in the adhesive. now i am hereing other stories from other tilers who have also had problems but bought the product elsewhere.😳
I can advise we virtually never have problems here with any of our brands and I am very experienced with the tecnical attributes of other normal brands & products but this is different & none of the common answers as to why it is happening apply & no answers are forthcoming from BASF here who don't normally handle tile & stone adhesives in this country & so are very little help, they are just keeping their fingers crossed that the problem goes away & it was all a big gliche or misunderstanding - but it isn't. :incazzato: and so i am attempted to finally get to the bottom of it for them.
what I can tell you is that in every case whether inside-outside or wall or floor to any substrate & with all tilers & various methods of application the 1 common denominator I can find is, in each case the problem tile has been porcelain - large 300x600 or 600x600 and large notched trowels or back buttering were used to make up for any uneveness in the substrate.
any suggestions will be graciuosly accepted but actual experience would be even better