J

J Sid

Turn ufh up to max and leave for a day, measure the floor surface temperature. Have to check, but the max allowed is about 28 Deg over the whole floor with a max of 35 degrees over a max of 1m2 (wetroom floor as an example).
Need to find out what happened before you fix again....
I would use Ditra rather than HB
 
W

WetSaw

Was the ply primed? Looks like the adhesive sucked into that before it stuck to the tiles.
 

kevsalt

TF
Esteemed
Arms
Reaction score
127
ribbs in the addy are still visible ...looks like minimum contact to the tile is a poss cause
 

Cris

TF
Reaction score
17
If tiles are porcelain there's a possibility that incorrect addy was used. Regular addy with no additive used ie porcelplus, can cause tiles to fail.... come across it in past. Especially if tiles were not back buttered
 

Reply to Failed Floor in the Australia area at TilersForums.com

Or checkout our tile courses and training forum or the Tile Blog / Latest Blog Posts

Please note that this thread is old so replying to it may not get a response. You'd be best posting a new thread with a good 4 or 5 word title.
This website is hosted and managed by www.untoldmedia.co.uk. Creating content since 2001.
Please visit our sponsor websites, they keep the forum free to use!
Tile Contractor Forum. The useful tile contractor website.

UK Tiling Forum Stats

Threads
67,370
Messages
881,207
Members
9,533
Latest member
laattaana
Top
AdBlock Detected

We get it, advertisements are annoying!

Sure, ad-blocking software does a great job at blocking ads, but it also blocks useful features of our website. For the best site experience please disable your AdBlocker.

I've Disabled AdBlock    No Thanks